•   0091-22-66157017
  •   info@torqbolt.com
  • Home

    ASTM F467/F467M Grade C63000 Alloy 630 Nuts Specification

    Heavy-duty aluminum bronze nuts engineered for industrial durability.

    ASTM F467/F467M Grade C63000 Alloy 630 Nuts provide excellent wear resistance, corrosion protection, and mechanical strength for offshore and engineering applications.

    ASTM F467/F467M Chemical Composition

    ASTM F467/F467M Copper and Copper-Base Alloys

    UNS Designation Number Alloy General Name Al Cu, min Fe, max Mn, max Ni, max P Si Zn, max A Pb, max Tin As, max
    ASTM F467/F467M Grade C63000 630 aluminum bronze 9.0- 11.0 78.0 D 2.0-4.0 1.5 4.0-5.5 . . . . . . 0.25 max . . . . . . 0.20 max
    • (A) Elements shown as balance shall be arithmetically computed by deducting the sum of the other named elements from 100.
    • (D) Minimum content of copper plus all other elements with specified limits shall be 99.5 %.

    ASTM F467/F467M Mechanical Requirements

    ASTM F467/F467M Mechanical Requirements (Inch)

    Alloy Mechanical Property Marking Hardness, min A Proof Stress, Hex Nut min, ksi Proof Stress, Heavy Hex Nut min, ksi B
    ASTM F467 Alloy Cu 630 F 467H 85 HRB 100 108
    • (B) Proof stress values for heavy hex nuts are based on 1.08 times the value for corresponding regular hex nuts.

    ASTM F467M Mechanical Requirements (Metric)

    Alloy Mechanical Property Marking Hardness, min A Proof Stress, Mpa
    ASTM F467M Cu 630 F467MH 85 HRB 690

    ASTM F467/F467M Tensile Stress Areas and Threads per Inch

    Nominal Size, in. Coarse Threads-UNC Fine Threads-UNF 8 Thread Series-8UN
    Threads/in. Stress Area A, in 2 Threads/in. Stress Area A, in 2 Threads/in. Stress Area A, in 2
    1/ 4 20 0.0318 28 0.0364 . . . . . .
    5/ 16 18 0.0524 24 0.0580 . . . . . .
    3/ 8 16 0.0775 24 0.0878 . . . . . .
    7/ 16 14 0.1063 20 0.1187 . . . . . .
    1/ 2 13 0.1419 20 0.1599 . . . . . .
    9/ 16 12 0.1820 18 0.2030 . . . . . .
    5/ 8 11 0.2260 18 0.2560 . . . . . .
    3/ 4 10 0.3340 16 0.3730 . . . . . .
    7/ 8 9 0.4620 14 0.5090 . . . . . .
    1 8 0.6060 12 0.6630 . . . . . .
    1 1/ 8 7 0.7630 12 0.8560 8 0.790
    1 1/ 4 7 0.9690 12 1.0730 8 1.000
    1 3/ 8 6 1.1550 12 1.3150 8 1.233
    1 1/ 2 6 1.4050 12 1.5810 8 1.492
    • (A) Tensile stress areas are computed using the following formula:
    • A s = 0.7854 [ D - 0.9743/n ]
      • where:
      • As = tensile stress area, in. 2 ,
      • D = nominal size (basic major diameter), in., and
      • n = number of threads per inch.

    ASTM F467/F467M Tensile Stress Areas and Threads per Metric

    Nominal Nut Diameter and Thread Pitch Stress Area, Amm 2 Nominal Nut Diameter and Thread Pitch Stress Area, Amm 2
    M6 × 1 20.1 M16 × 2 157
    M8 × 1.25 36.6 M20 × 2.5 245
    M10 × 1.5 58.0 M24 × 3 353
    M12 × 1.75 84.3 M30 × 3.5 561
    M14 × 2 115 M36 × 4 817
    • (A) Tensile stress areas are computed using the following formula:
    • As = 0.7854 (D − 0.9382P) 2
      • where:
      • As = tensile stress area, mm. 2 ,
      • D = nominal size (basic major diameter), mm., and
      • n = number of threads per mm.

    ASTM F467/F467M Heat Treatment

    Alloy Condition
    Copper (all alloys) As formed or stress relieved at manufacturer's option
    Nickel alloys 400 and 405 As formed or stress relieved at manufacturer's option
    Nickel alloy 500 Solution annealed and aged
    Aluminum alloy 2024-T4 Solution treated and naturally aged
    Aluminum alloy 6061-T6 Solution treated and artificially aged
    Aluminum alloy 6262-T9 Solution treated, artificially aged, and cold worked
    Titanium 625 Annealed

    Frequently Asked Questions

    What is Nickel-Aluminum Bronze C63000?

    Nickel-aluminum bronze C63000 (NAB) is a Cu-Al-Ni-Fe alloy (~82 Cu, 9.5 Al, 5 Ni, 4 Fe) per ASTM F467 - the premium aluminum bronze for marine + severe service bolting. Tensile 90-115 ksi, yield 50-70 ksi. The workhorse marine pump + propeller nut alloy.

    Where is C63000 used?

    Marine propeller hardware, pump impeller shaft bolts, naval shipboard bolting, desalination plant fasteners, and any seawater service requiring high strength + cavitation resistance + galvanic compatibility with bronze workpieces. The standard high-strength marine bronze.

    How does C63000 compare to cupro-nickel C71500?

    C63000 is stronger but heavier; C71500 has better resistance to ammoniacal seawater corrosion and is the preferred alloy for condenser tube-sheet nut in some chemistries. C63000 is the structural marine fastener; C71500 is the heat-exchanger fastener.

    Available dimensional patterns?

    Full F467 range - ASME B16.5 flange studs (marine valve bolting), B18.2.1 hex cap screws, B18.3 socket head, B18.31.2 clamping studs. Highest-volume nickel-aluminum bronze fastener spec.

    References & Standards

    • ASTM F467 / F467M - Standard Specification for Nonferrous Nuts for General Use
    • ASTM F468 / F468M - Companion specification for Nonferrous Bolts, Hex Cap Screws, and Studs (mate with F467 nuts for matched-alloy assemblies)
    • ASTM F436 / F436M - Hardened steel washers (ferrous washer companion when nonferrous washers are not specified)
    • NACE MR0175 / ISO 15156 - Sour-service hardness limits for petroleum and natural gas industries
    • ASME B18.2.2 / B18.2.4.1M / B18.2.4.6M and ISO 4032 / 4033 / 4035 - Dimensional standards referenced by F467
    • DIN 934 / 439 / 6330 - Metric hex nut dimensional standards